AicaigouB2B Wiki

ZG35Cr24Ni7N Heat-resistant Alloy Cast Steel

Updated: 2026-10-20

Overview

ZG35Cr24Ni7N is a specially formulated heat-resistant cast steel designed for prolonged service at elevated temperatures. The alloy designation indicates its chemical composition, containing approximately 35% chromium (Cr), 24% chromium (Cr), and 7% nickel (Ni), with nitrogen (N) addition for enhanced high-temperature properties. This material was developed specifically for industrial applications where components must maintain structural integrity in continuous high-temperature environments, typically between 900°C and 1100°C. The balanced composition provides optimal resistance to oxidation, creep deformation, and thermal fatigue, making it superior to standard stainless steels in severe thermal conditions.

Physical and Chemical Properties

ZG35Cr24Ni7N exhibits exceptional high-temperature stability due to its chromium-rich matrix that forms a protective oxide layer. At room temperature, it demonstrates typical tensile strength of 450-550 MPa, which remains relatively stable up to operating temperatures. The nickel content enhances ductility and thermal shock resistance. The alloy's microstructure remains stable under prolonged heat exposure, resisting the formation of detrimental sigma phase precipitation common in high-chromium alloys. Its thermal expansion coefficient is approximately 15-16 μm/m·°C in the 20-1000°C range. The nitrogen addition improves creep rupture strength and stabilizes the austenitic structure at elevated temperatures.

Main Applications

The primary use of ZG35Cr24Ni7N is in manufacturing furnace components for heat treatment and metal processing industries. Common applications include radiant tubes, muffles, furnace rollers, and hearth plates in continuous annealing lines. The power generation industry utilizes this alloy for burner nozzles, cyclone separators, and other boiler components exposed to combustion environments. In chemical processing, it serves in pyrolysis furnace parts and reforming furnace tubes. The material is particularly valued for batch furnace fixtures that undergo repeated thermal cycling. Compared to standard heat-resistant alloys, ZG35Cr24Ni7N offers extended service life in oxidizing atmospheres up to 1150°C and carburizing atmospheres up to 1050°C.

Safety and Storage

While ZG35Cr24Ni7N doesn't present special toxicity concerns beyond standard steel alloys, precautions should be taken during machining. Grinding and welding operations require proper ventilation to control metal fume exposure. The material should be stored indoors in low-humidity conditions to prevent surface contamination. Preheating is recommended before welding (200-300°C) and slow cooling afterward to minimize thermal stresses. Finished components should be protected from chloride contamination during storage, as localized corrosion can occur despite the alloy's generally good corrosion resistance. Handling should follow standard industrial safety protocols including eye protection and gloves for sharp edges.

B2B Procurement Guide

When procuring ZG35Cr24Ni7N components, clearly specify the required heat treatment condition (typically solution annealed), dimensional tolerances, and any special surface finish requirements. For critical applications, request material certification including chemical analysis and mechanical property test reports. Lead times for cast components can be significant (8-12 weeks commonly), so plan procurement accordingly. Consider working with foundries that specialize in high-temperature alloys for optimal quality. Pricing for raw castings typically follows weight-based models, while machined components are priced based on complexity. For reference, raw casting prices typically range from $3.50 to $6.00 per kilogram depending on order volume and complexity.