Iron-based Superalloy
Overview
Iron-based Superalloys are advanced metallic materials engineered to maintain structural integrity under extreme conditions exceeding 600°C. Developed as a cost-effective alternative to nickel-based superalloys, they combine iron with chromium, nickel, and other alloying elements to achieve exceptional high-temperature performance. These alloys are particularly valued in industries where materials must withstand prolonged exposure to thermal stress, oxidation, and mechanical loads. While not matching nickel alloys in maximum temperature capability, iron-based variants offer superior cost-efficiency for many mid-range applications.
Physical and Chemical Properties
The microstructure of iron-based superalloys typically consists of an austenitic matrix strengthened by various precipitate phases. Chromium content (15-25%) provides oxidation resistance, while additions of aluminum and silicon further enhance scaling resistance at high temperatures. Mechanical properties include tensile strengths of 500-1000 MPa at room temperature, maintaining 200-400 MPa at 700°C. Thermal expansion coefficients range from 12-18 μm/m·°C, with thermal conductivity of 15-25 W/m·K. The alloys demonstrate excellent creep rupture life, often exceeding 100 hours at 650°C under 100 MPa stress.
Main Applications
In aerospace, these alloys are used for turbine disks, compressor components, and afterburner parts where temperatures stay below 750°C. Power generation applications include steam turbine blades, boiler tubes, and heat exchangers in fossil fuel plants. The petrochemical industry utilizes them for catalytic converter housings and pyrolysis furnace components. Emerging applications include concentrated solar power systems and advanced nuclear reactor designs where cost-effective high-temperature materials are critical.
Safety and Storage
As manufactured products, iron-based superalloys present minimal health risks. However, machining operations require dust control measures as metal particulates may cause respiratory irritation. Proper ventilation and PPE (N95 masks) are recommended during grinding or cutting processes. Storage should prevent galvanic corrosion by separating from dissimilar metals in humid environments. Bulk material is typically supplied with protective coatings or in sealed containers to prevent surface oxidation during transit and warehousing.
B2B Procurement Guide
Industrial buyers should clearly specify mechanical property requirements (tensile strength, creep life), maximum service temperature, and environmental conditions (presence of sulfur, salt, etc.). Standard forms include billets, bars, plates, and custom castings, with lead times varying from weeks for stock items to months for specialized compositions. Quality certifications to request include material test reports (MTRs) with chemical analysis and mechanical test data. For critical applications, additional NDE (non-destructive examination) such as ultrasonic testing may be specified. Major global suppliers include Special Metals Corporation, Haynes International, and Hitachi Metals.
Related Manufacturers
- 主营:--
- 主营:--
- 主营:--
- 主营:Inconel 718、Hastelloy C276、Monel400、高温合金、哈氏合金、蒙耐尔合金、精密合金、Inconel X750、Inconel625、Incoloy 825、Haynes188、Haynes 25、GH3030、GH5188、GH3625、GH3536、GH2132、GH3044、GH4145、GH3600、GH3039、Alloy 20、Alloy28、GH4169圆钢
- 主营:铝板、铝棒、铝管、高温合金、钛合金、模具钢
- 主营:高温合金钢板 圆棒、镍基合金钢管
- 主营:中厚板、氩弧焊、无缝管、温合金、镍合金、硅合金、合金板、膨胀合金、耐蚀合金、耐热合金、哈氏合金、合金材料、镍基合金、导磁合金、铍封合金、软磁合金、弹性合金、镍基焊丝、锻带线材、锻环精车、镍基焊材、精密铸件、特殊钢材、圆棒板材、高温螺栓
- 主营:哈氏合金、高温合金、特种合金、lnconel合金、lncoloy合金、精密合金、monel合金、司太立合金、铜镍合金、铜及铜合金
- 主营:板切割、无缝管、inconel625、合金管、哈氏合金、合金钢板、耐热圆棒、不锈钢板、耐磨铸件、对焊法兰、钢板材料、不锈钢管、离心铸管、平焊法兰、钢板检测、圆棒锻造、光亮圆棒、无缝钢管、高温钢板、铸造料架、弯头管件、钢板板材、圆钢切割、不锈圆钢、圆棒切割
- 主营:c70600
- 主营:金属硅、金属硅粉、单质硅粉、工业硅、工业硅粉
- 主营:钴基焊丝、铸铁焊条、药芯焊丝用焊芯、镶嵌合金锤头、高铬合金锤头、超耐磨复合颗粒锤头、纯镍粉末、镍基粉末、不锈钢粉末、双金属复合锤头、板锤、筛板、衬板、鄂板、破碎机配件、破碎机甩锤
- 主营:镍基合金、高温合金、铜镍合金
- 主营:光亮线、结构钢、铝棒材、镍基合金、精密合金、高温合金、超级不锈钢、合金钢、铍铜棒、棒管件、大圆棒、板棒管、铍青铜、钛棒管、热轧板、车光棒、钛板棒、钢带材、航空铝、无缝管、纯钛板、冷轧板
- 主营:硒粉、镍粉、硅粉、高纯铁合金粉、铜粉、钨粉、二氧化锡、钼粉、锡粉、银粉、碳化钨
- 主营:热轧棒、精密棒、圆钢棒材、磁合金、合金棒、铁基合金、高温合金、合金圆钢棒、精密铸件
- 主营:感应熔炼、4822、钛铝、合金靶材、中间合金、高温合金、高熵合金、难熔合金、钛合金、铝合金、镁合金、铜合金、镍合金、钴合金、铌合金、锆合金、镍基合金、实验钢、熔炼钛铝、钴铬钼、铝铌、TNM、悬浮熔炼、镍钛、高纯铝
- 主营:马氏体时效钢、GH5188、GH3625、航空专用合金、高温合金、钴基合金、1J22钴基合金、4J29可伐合金、GH4169、L605、GH4099、叶片钢、PH13-8Mo、Aermet100、GH5605、1J22、18Ni300、18Ni350、Monel400、MP159、MP35N、3J21、GH2747、18Ni250
- 主营:分析仪、金属铁、碳化钛、各种牌号铁基合金粉末、金属铋、金属铌、防爆管、喷涂粉、铝铸件、铜铁铝、脱氧铝、铋粉末、纯铋粉、疏通剂、粗铜粉、纯银粒、细镍粉、电解镍、铁粉末、紫铜粒、铌铁粉、氧化铁、氧化铬、金属锡、纯钨粉、钼圆柱
- 主营:高温合金、镍基合金、哈氏合金、哈氏合金 C276、镍基合金板、镍基合金管、Incoloy800H、不锈钢无缝管
- 主营:铝型材、空心管、铝方管、铝合金、镁合金、镍合金、合金板、合金管、铝管材、铝圆管、铝锻管、圆棒管、研磨棒、铝棒材、拉丝板、铝板带、铝线槽、船舶板、铝板材、无缝管、铝方棒、铝单板、铝锻件、布线槽、护栏管
- 主营:锡锭、铅锭、锑锭、铁合金、铝合金、铜合金、zl102铝合金锭、钼条、铋锭、铟锭、镁锭、海绵钛、金属硅、电解锰、金属铬、镉锭、海绵锆、高纯镁锭、阴极铜、铝锭、锌锭、高碳锰铁、6063铝棒
- 主营:银焊条、银焊丝、铜焊条、耐热钢焊条、耐热钢焊丝、铜焊丝、铝焊条、铝焊丝、耐磨焊条、耐磨焊丝、堆焊焊条、堆焊焊丝、不锈钢焊条、不锈钢焊丝、低温钢焊条、低温钢焊丝、防水焊条、药心焊丝、氩弧焊丝、埋弧焊丝
- 主营:抓斗、炉底板、落煤管、铁基高温合金GH1131钢板、离心铸管、垫铁炉枕、吊具、料框、料盘、坩埚、滑块、高铬铸板、炉辊、溜渣槽、钢板、无缝管、圆棒